下面就濟(jì)南抹面砂漿施工中導(dǎo)致外墻保溫系統(tǒng)抹灰砂漿層裂縫的施工因素進(jìn)行分析。
Next, the paper analyzes the construction factors that cause the cracks in the plastering mortar layer of the external wall insulation system in the plastering mortar construction of Jinan.
外墻外保溫系統(tǒng)在本工程施工現(xiàn)場(chǎng)完成。抹面砂漿的質(zhì)量關(guān)系到保溫系統(tǒng)的整體質(zhì)量,也是導(dǎo)致保溫抹灰砂漿層開(kāi)裂的重要因素。
The external wall external insulation system shall be completed at the construction site of the project. The quality of plastering mortar is related to the overall quality of the insulation system, and it is also an important factor leading to the cracking of the insulation plastering mortar layer.
1. 基礎(chǔ)面平整度偏差過(guò)大,調(diào)整粘結(jié)劑厚度、調(diào)整多層板、調(diào)整表面拋光、調(diào)平等,都會(huì)導(dǎo)致保溫質(zhì)量的質(zhì)量缺陷。
1. If the flatness deviation of the foundation surface is too large, adjusting the thickness of the binder, adjusting the multi-layer plate, adjusting the surface polishing, and adjusting the equality will lead to the quality defects of the insulation quality.
2、基層表面含有粉塵等阻礙膏體的物質(zhì),膏體制作時(shí)未進(jìn)行界面處理。
2、 The surface of the base layer contains dust and other substances that hinder the paste, and the interface treatment is not carried out when the paste is made.
3.濟(jì)南粘接砂漿介紹保溫板粘接面積太小,不符合規(guī)范和施工方案的要求,不能滿足粘接面積的質(zhì)量要求。
3. Jinan bonding mortar introduces that the bonding area of insulation board is too small, which does not meet the requirements of specifications and construction scheme, and cannot meet the quality requirements of bonding area.
4. 保溫板的埋深和錨釘數(shù)量不符合設(shè)計(jì)和施工方案的要求。
4. The buried depth of the insulation board and the number of anchor nails do not meet the requirements of the design and construction scheme.
5. 耐堿性玻璃纖維網(wǎng)格布的研磨寬度不符合規(guī)范要求,研磨處產(chǎn)生裂紋。
5. The grinding width of alkali resistant glass fiber mesh does not meet the specification requirements, and cracks are produced at the grinding place.
6. 門(mén)窗開(kāi)口的四個(gè)角是應(yīng)力集中的地方。沿門(mén)窗開(kāi)口45°方向不加耐堿玻纖網(wǎng)布,經(jīng)常出現(xiàn)裂縫。
6. The four corners of the door and window opening are the places where the stress is concentrated. Along the 45 ° direction of the door and window opening, alkali resistant glass fiber mesh is not added, and cracks often occur.
7. 在太陽(yáng)暴曬或高溫天氣下施工抹灰砂漿層,保水性能不足,導(dǎo)致抹灰砂漿層失水過(guò)多而產(chǎn)生裂縫。
7. When the plastering mortar layer is constructed in the sun or high temperature weather, the water retention performance is insufficient, resulting in excessive water loss of the plastering mortar layer and cracks.
濟(jì)南抹面砂漿介紹了導(dǎo)致外墻保溫系統(tǒng)抹灰砂漿層裂縫預(yù)防措施的材料因素
Jinan plastering mortar introduces the material factors that cause the cracks in the plastering mortar layer of the external wall insulation system
1、圖紙?jiān)O(shè)計(jì)選擇密度18 - 22公斤/立方米保溫板,材料的批準(zhǔn)由國(guó)家檢驗(yàn)機(jī)構(gòu)檢驗(yàn)合格,保溫材料進(jìn)入現(xiàn)場(chǎng)測(cè)量后質(zhì)量檢查的密度,在施工的過(guò)程中檢查或定期聚苯板測(cè)量密度,防止施工單位在施工過(guò)程中以次充好的行為。
1. The density of 18-22kg / m3 insulation board is selected in the drawing design. The approval of the material is inspected and qualified by the national inspection agency. The density of the quality inspection after the insulation material enters the site for measurement. During the construction process, check or regularly measure the density of polystyrene board to prevent the construction unit from shoddy behavior in the construction process.
2. 保溫材料應(yīng)由系統(tǒng)材料供應(yīng)商配套供應(yīng),充分發(fā)揮粘結(jié)劑、保溫板、耐堿玻璃纖維網(wǎng)布、抹灰砂漿的整體效果。
2. The thermal insulation material shall be supplied by the system material supplier to give full play to the overall effect of binder, thermal insulation board, alkali resistant glass fiber mesh and plastering mortar.
3、濟(jì)南抹面砂漿告訴你選擇正常施工企業(yè)綜合實(shí)力盡可能開(kāi)發(fā)人員可以支付預(yù)付款prematerial,建設(shè)單位必須需要提前定制保溫板,為了確保保溫板保溫施工前有足夠的老化時(shí)間,防止墻后的保溫板繼續(xù)萎縮。
3. Jinan plastering mortar tells you to choose the normal construction enterprise's comprehensive strength as much as possible, the developer can pay the advance payment, the construction unit must customize the insulation board in advance, in order to ensure that the insulation board has enough aging time before construction, to prevent the insulation board behind the wall from shrinking.
4、將聚苯乙烯板糊固定好后,其糊強(qiáng)度要滿足要求,及時(shí)做好表面層,避免因曝光時(shí)間過(guò)長(zhǎng)而引起的板面溫度過(guò)高。
4. After the polystyrene board paste is fixed, the paste strength shall meet the requirements, and the surface layer shall be prepared in time to avoid the board temperature caused by too long exposure time.
5. 基礎(chǔ)與粘結(jié)劑的抗拉結(jié)合強(qiáng)度不低于0.3mpa,結(jié)合界面分離面積不大于50%。
5. The tensile bond strength of foundation and binder shall not be less than 0.3mpa The separation area of the interface shall not be greater than 50%.
6. 外墻保溫系統(tǒng)的材料應(yīng)符合《發(fā)泡聚苯板薄抹灰外墻保溫系統(tǒng)》、《外墻保溫工程技術(shù)規(guī)程》等相關(guān)行業(yè)標(biāo)準(zhǔn)的要求。
6. The materials of external wall insulation system shall meet the requirements of relevant industry standards such as foamed polystyrene board thin plastering external wall insulation system, technical specification for external wall insulation engineering, etc.